EUROSUPERALLOYS 2014
2nd European Symposium on Superalloys and their Applications
12 –16 May, 2014, French Riviera, Giens, France
Posters available
Posters listed below may be downloaded: double click on the title
Precipitation
0042
Metallurgical Optimization of PM Superalloy N19
Didier Locq1, Loïc Nazé2, Jean-Michel Franchet3, Pierre Caron1, Alice
Dumont2, Alain Köster2, Jean-Yves Guédou4
1Onera – The French Aerospace Lab, Châtillon, FR, 2CdM Mines ParisTech,
Evry, FR, 3Snecma-SAFRAN Group, Colombes, FR, 4Snecma-SAFRAN Group,
Moissy-Cramayel, FR
0151
High Resolution Orientation Mapping of Secondary Phases in ATI 718Plus®
Robert Krakow1, Mark C. Hardy2, Catherine M.F. Rae1, Paul A. Midgley1
1University of Cambridge, Cambridge, GB, 2Rolls-Royce plc, Derby, GB
0173
Examination of Chemical Elements Partitioning between the
g and g' Phases in
CMSX-4 Superalloy using EDS microanalysis and electron tomography methods
Beata Dubiel, A. Kruk, A. Czyrska-Filemonowicz
AGH University of Science and Technology, Krakow, PL
Process Microstructure interactions
Alexander Echin, Yury Bondarenko
FSUE “All Russian Scientific Research Institute of Aviation Materials (VIAM)”, Moscow, RU
0027 Selective Electron Beam Melting of CMSX-4
Carolin Körner, Markus Ramsperger University of Erlangen-Nuremberg, Erlangen, DE
Dexin Ma1, Jianping Hong1, Fu Wang1, Bührig-Polaczek Andreas
1 1RWTH, Aachen, DE, 2Shanghai Jiao Tong University, Shanghai, CN, 3Northwestern Polytechnical University, Xi’an, CN
Fu Wang, Dexin Ma, Hao Lu, Andreas Bührig-Polaczek RWTH, Aachen, DE
0081 Thermal History Prediction Modelling Tool for Investment Casting
Laura Maestro1, Aitor Eguidazu1, Iñaki Vicario1, Jose Agustín Torroba2, Efrain Morelli2, Ole Koeser4, Andrea Carosi3
1Precicast Bilbao S.A, Barakaldo, ES, 2University of Applied Sciences and Arts, Sion, CH, 3Precicast Novazzano S.A, Novazzano, CH, 4Calcom ESI S.A, Lausanne, CH
0138 Effect of solidification parameters on the dendrite arm spacing in MAR M-247
Srdjan Milenkovic1, Mehdi Rahimian1, Ilchat Sabirov1, Laura Maestro2 1IMDEA Materials Institute, Getafe, ES, 2Precicast Bilbao, S.A., Bilbao, ES
0160 Weldability of Superalloys Haynes 188 and Hastelloy X by Nd: YAG Laser
Jérémie Graneix, Yannick Balcaen, Jean-Denis Beguin, Joel Alexis, Talal Masri Université de Toulouse, Tarbes, FR
Recrystallisation and grain growth
0018
Multipass Forging of Inconel 718 in the Delta-Supersolvus Domain: Assessing
and Modeling Microstructure Evolution
Meriem Zouari2, Sébastien Rousselle1, Nathalie Bozzolo1, Roland Logé1
1CEMEF Mines ParisTech, Sophia Antipolis, FR, 2Manoir Aerospace-Forges De
Bologne, Chaumont, FR
Mechanical behavior
Octavio Covarrubias1,2 1Frisa Forjados SA de CV, Santa Catarina, Mexico, 2Universidad Autonoma de Nuevo Leon, San Nicolas, Mexico
0013
Impact of Microstructural Evolutions during Thermal Aging of Alloy 625 on
its Static Mechanical Properties
Lorena Mataveli Suave1, Denis Bertheau1, Jonathan Cormier1, Patrick
Villechaise1, Aurélie Soula2, Zéline Hervier3, Johanne Laigo4
1Institut Pprime, Chasseneuil, FR, 2Aircelle – SAFRAN Group, Plaisir, FR,
3Turbomeca – SAFRAN Group, Bordes, FR, 4Snecma – SAFRAN Group,
Moissy-Cramayel, FR
0014
Development and Use of a New Burner Rig Facility to Mimic Service Loading
Conditions of Ni-Based Single Crystal Superalloys
Florent Mauget1, Damien Marchand1, Médéric Morisset1, Denis Bertheau1,
Jonathan Cormier1, José Mendez1, éline Hervier2, Elisabeth
Ostoja-Kuczynski2
1Institut Pprime, Chasseneuil, FR, 2SAFRAN - Turbomeca, Bordes, FR
0041
Quantitive analysis of Portevin -Le Chatelier effect in Inconel 718 at
elevated temperatures
Jaroslaw izera , Warsaw University of technology, Warsaw
142
Creep-Fatigue Interactions in Equiaxed and Single Crystal Ni Based
Superalloys
Erica Vacchieri1, lessio Costa1, Eleonora Poggio1, Stuart Richard
Holdsworth2
1Ansaldo Energia S.p.A., Genoa, IT, 2EMPA Swiss Federal Laboratories for
Materials Science and Technology, Dübendorf, CH
Native defects and precipitate evolution in single crystals
0072 The role of Particle Ripening in Accelerating the Creep of Nimonic 263
Giuliano Angella, Riccardo Donnini, Maurizio Maldini, Dario Ripamonti CNR-IENI, Milan, IT
Deformation and damage mechanisms
Kang Yuan1, Ru Lin Peng1, Xin-Hai Li2, Sten Johansson1, Yan-Dong Wang3
1Linköping University, Linköping, SE, 2Siemens Industrial Turbomachinery AB, Finspång, SE, 3University of Science and Technology Beijing, Beijing, CN
0168 Observation of Dislocation Evolution during Straining of a g-g’ Superalloy Single Crystal using the CECCI technique.
Stefan Zaefferer1, Zailing Zhu2, Roger Reed2
1Max-Planck-Institut für Eisenforschung, Düsseldorf, DE, 2University of Oxford, Oxford, GB
Alloy development
0010 Development of Advanced P/M Ni-Base Superalloys for Turbine Disks
Gerhikh Garibov, Nina Grits, Alexey Vostrikov, Elizaveta Fedorenko, Alexander Volkov, All-Russia Institute of Light Alloys Stock Co., Moscow, RU
0037 New Single Crystal Superalloys - Overview and Update
Jacqueline Wahl, Ken Harris, Cannon-Muskegon Corporation, Muskegon, USA
0164 Microstructure Stability Optimization of 263 Ni-Based Superalloy
Coraline Crozet, Alexandre Devaux, Denis Béchet, Aubert & Duval, Les Ancizes, FR
0214 HAYNES 244 alloy - a New 760°C Capable Low Thermal Expansion Alloy
Michael Fahrmann, Lee Pike Haynes International Inc., Kokomo, USA